- Turning of Bohler steel 390 mocroclean
-
Hello
I have to turn a lot of bead parts.
The most of roughing work is from Dm 73 to Dm 32x 75lg.
I made a test, 150m with 0,354f and from 2mm
The plate got it (was already tightly worn out)
Plate CNMM 120408 P25 normal edge honing, rather sharp.
Who has a tip or any experienced data?
Regards, Baconpep
-
-
Can’t anybody tell anything?
A tip?
Regards, Baconpep