any guidance appreciated mach thin 6/8 mm plates avg . 6X8" weldments . super duplex warps & is very abrasive on tools .especially after welding. I only have approx 1mm to clean up both sides & w/ welded spots it really chews up tools. am using carbide inserts for finish cuts .005 or less;and am using corncob mill to rough . which is a relative term because .020 is about as deep as i can go without destroying tool. any hints out there ???