What would the equation be for release of Cr+6 ions into the air from cutting metal, either with heat or with tools? Just because 'chromium' is present doesn't mean there is any provable risk if the sequence that produces it is highly improbable under ordinary conditions.
Indeed, is chrome as an alloy in a hexavalent state within the mix?
__________________ First you get good, then you get fast. Then grouchiness sets in.