for my anodizing I use a vibratory tumbler with the 1/4" plastic triangles to remove machine marks (i use the green ones), it will leave a matte finish. From here I then run it in walnut shells with rouge for about 36 hours. It brings the part to a very high shine. Since I want my anodized parts to look almost translucent I need to have a high polish before they go into the tanks... |