I haven't see it. This picture even shows a little tit in the middle where the end mills center wasn't cutting. I am shooting 15% GFPP, works good. Now this is a steel core, I tried to take pictures on an aluminum one, to shinny, couldn't get a clear picture. I am not saying subgates that have all the proper angles in them do not have a place, but from what I have seen of other mold makers work , I have not seen any that have done it the text book way. All have their own little spin. Also with the aluminum, the sub gates running GF does tend to wear on them, so I mainly use for low volume or put a steel insert in for the gate. |